产品展示 | 联系双虎 |

欢迎访问济南双虎围挡厂官网!

经理

13953162123

您先的位置:首页 > 新闻资讯 > 公司新闻

公司新闻

济南彩钢板房防火涂料施工应满足的条件

文章发布: 发表时间:2017-07-18 10:23:52

1.济南彩钢板房防火喷涂维护应由经过培训合格的专业施工队施工。施工中的安全技能和劳动维护等请求,应按国家现行有关规定履行。
1. Ji'nan color steel house fire spraying maintenance should be trained through the construction of professional construction team. The safety skills and labor maintenance shall be fulfilled in accordance with the relevant regulations of the state.
2.当济南彩钢板房装置就位,与其相连的吊杆、马道、管架及别的相干系的构件装置结束,并经检验合格后,方可进行防火涂料施工。
2. when the Ji'nan steel housing unit in position, pipe rack and other structural devices correlated boom, Ma Road, connected with the end, and after inspection, construction can fire coatings.
3.施工前,济南彩钢板房外表应除锈,并依据运用请求确定防锈处理。除锈和防锈处理应契合现行《钢结构工程施工与检验规范》中有关规定。
3. before construction, the surface of Ji'nan color steel board room should be rust removed, and the rust prevention treatment shall be determined according to the application requirements. Rust removal and rust prevention treatment shall be in accordance with the relevant provisions in the current regulations on construction and inspection of steel structures.
4.济南彩钢板房 http://www.jnjinrun.com/ 外表的杂物应铲除洁净,其衔接处的缝隙使用防火涂料或别的防火资料添补堵平后方可施工。
4. Ji'nan steel housing surface debris should be removed clean, the connecting point of the gaps in the use of fire retardant coating or other materials to fill fire wall before construction.
5.施工防火涂料应在室内装饰之前和不被后继工程所损坏的条件下进行。施工时,对不需作防火维护的部位和别的物件应进行遮盖维护,刚施工的涂层,应防止脏液污染和机械撞击。
5. construction fire retardant coating should be before interior decoration and not damaged by subsequent projects. During construction, cover and other objects that do not need fire protection shall be covered and maintained, and the coating for the construction shall be protected against dirty liquid pollution and mechanical impact.
6.施工进程中和涂层枯燥固化前,环境温度宜保持在5~38℃,相对湿度不宜大于90%,空气应流转。当风速大于5m/s,或雨天和构件外表有结露时,不宜工作。
6. the construction process and coating dry before curing, the ambient temperature should be maintained at 5 to 38 DEG C, relative humidity should not be greater than 90%, the air flow. It is not suitable to work when wind speed is greater than 5m/s, or when rainy weather and condensation of components appear.